陈达上. 1993. 谈谈涂料的粉化问题. 施工技术与管理,(4): 30-32.
林鹏凌, 杜爱琴, 邹华彬. 2005. 凝胶渗透色谱法测定聚氨酯树脂的平均相对分子质量. 化学分析计量,14(3): 40-41.
(Lin P L, Du A Q, Zou H B. 2005. Mean relative molecular weight determination of polyurethane resin by gpc. Chemical Analysis and Meterage, 14(3): 40-41. [in Chinese] )
刘登良. 2003. 涂层失效分析的方法和工作程序. 北京:化学工业出版社.
刘 毅, 郭洪武, 左 静, 等. 2012. 纳米TiO2改性涂料涂饰染色单板的光变色. 林业实用技术,(11):97-99.
龙 玲, 万祥龙, 王启宝, 等. 2010. 纳米TiO2对水性木器漆涂饰单板耐光色牢度的影响. 木材工业, 24(1):11-14.
(Long L, Wan X L, Wang Q B, et al. 2010. Color fastness of veneer with Nano-TiO2 modified waterborne coating. China Wood Industry, 24(1):11-14. [in Chinese] )
龙 玲, 万祥龙, 曲岩春. 2011. 纳米Al2O3改性水性木器漆耐磨性和硬度的研究. 林业科学, 49(9):108-113.
(Long L, Wan X L, Qu Y C. 2011. Study on wearing resistance and hardness of the Nano-Al2O3 modified waterborne wood coating. Scientia Silvae Sinicae, 49(9):108-113. [in Chinese] )
楼 淼,胡永乐,强文江,等.2010.洞室环境钢结构防腐及涂层起泡分析.涂料工业,40(11):35-37.
(Lou M, Hu Y L, Qiang W J, et al. 2010. Analysis in blistering of anticorrosion coatings for steel structure in grotto environment. Paint & Coatings Industry, 40(11):35-37. [in Chinese] )
陆步云,Merlin A, Perre P, 等. 2007. 室外涂饰木材的抗老化性能. 南京林业大学学报: 自然科学版, 31(4): 61-64.
(Lu B Y, Merlin A, Perre P, et al. 2007. Research on anti-aging ability of exterior coated wood. Journal of Nanjing Forestry University(Natural Sciences Edition), 31(4): 61-64. [in Chinese] )
莫引优, 陈 奎, 何其飞, 等. 2012. 用二氧化硅聚氨酯涂料改良木材表面性质的研究. 北京林业大学学报, 34(4): 154-159.
(Mo Y Y, Chen K, He Q F, et al. 2012. Modifying wood surface properties by SiO2 polyurethane coating. Journal of Beijing Forestry University, 34(4): 154-159. [in Chinese] )
孙建琴. 2009. 色谱技术的分析比较及其新发展趋势. 凯里学院学报, 27(6): 41-44.
孙廷耀. 1999. 涂层起泡探析. 涂料工业,(3): 41-42.
(Sun T Y. 1999. Preliminary discussion on blistering of paint film. Paint & Coatings Industry, (3): 41-42. [in Chinese] )
王明瑞, 姬 红. 2010. 涂料涂膜失光的影响因素分析. 辽宁化工, 39(3): 310-311.
(Wang M R, Ji H. 2010. Analysis of influencing factors on glossiness loss of paint coating. Liaoning Chemical Industry, 39(3): 310-311. [in Chinese] )
王跃波, 钟宏伟, 朱红专. 2011. 金属涂层失效机制及其对策. 四川建材, 37(159): 30-31.
(Wang Y B, Zhong H W, Zhu H Z. 2011. Metal coating failure mechanism and countermeasures. Sichuan Building Materials, 37(159): 30-31. [in Chinese] )
伍忠岳,叶荣森.2009.纳米硅溶胶在水性木器涂料中的应用.中国涂料,(5):64-66.
(Wu Z Y, Ye R S. 2009. Use of nano silicasol in water-borne wood coatings. China Coatings, (5):64-66. [in Chinese] )
阎 瑞, 耿 志, 吴 行, 等. 2005. 潜艇表面涂层失效机理的研究. 海军工程大学学报, 17(5): 38-42.
(Yan R, Geng Z, Wu H, et al. 2005. On failure mechanism of submarine surface coatings. Journal of Naval University of Engineering, 17(5): 38-42. [in Chinese] )
朱福海. 1999. 高分子材料光降解和光稳定. 合成材料老化与应用,(1): 24-26.
朱则刚. 2012. 汽车涂装表面失光的原因分析及其处理. 涂料与应用,(2): 33-37.
Bardage S. 1998. Susceptibility of painted wood to Aureobasidium pullulans: fungal stain and growth patterns. Holz Roh Werkst, 56: 359-364.
Bayer G T, Zamanzadeh M.2004.Failure analysis of paints and coating.Matco Associates,Inc Pittsburgh,Pennsylvania.
Browne F L. 1958. Wood properties that affect paint performance. Madison, Wis.: US Dept of Agriculture, Forest Service, Forest Products Laboratory.
Bulcke J V, Acker J V, Stevens M. 2008. Experimental and theoretical behavior of exterior wood coatings subjected to artificial weathering. Journal of Coatings Technology and Research, 5(2): 221-231.
Bulcke J, Boone M, Acker J V, et al. 2010. High-resolution X-ray imaging and analysis of coatings on and in wood. Journal of Coatings Technology and Research, 7(2): 271-277.
Bull S J, Berasetegui E G. 2006. An overview of the potential of quantitative coating adhesion measurement by scratch testing. Tribology International, 39(2): 99-114.
Bussjaeger S, Daisey G, Simmons R, et al. 1999. Mildew and mildew control for wood surfaces. Coat Technol, 71(890): 67-69.
Cassens D L, Feist W C. 1991. Exterior wood in the south: Selection, application and finishes. Gen Tech Rep FPL-GTR-69, Madison WI: USDA, Forest Service, Forest Products Laboratory, 60.
Chang S T, Chou P L. 1999. Photo-discoloration of UV-curable acrylic coatings and the underlying wood. Polymer Degradation and Stability, 63(3): 435-439.
Chang S T, Hon N S, Feist W C. 1982. Photodegradation and photoprotection of wood surfaces. Wood Fiber Sci, 14: 104-117.
Dawson B S W, Singh A P, Kroese H W, et al. 2008. Enhancing exterior performance of clear coatings through photostabilization of wood. Part 2: coating and weathering performance. Journal of Coatings Technology and Research, 5(2): 207-219.
Derbyshire H, Miller E R.1981. The photodegradation of wood during solar irradiation. Holz ats Roh-und Werkstoff, 39: 341-350.
Doménech-Carbó M T, Yusá-Marco D J, Bitossi G, et al. 2008. Study of ageing of ketone resins used as picture varnishes by FTIR spectroscopy, UV-Vis spectrophotometry, atomic force microscopy and scanning electron microscopy X-ray microanalysis. Anal Bioanal Chem, 391:1351-1359.
Duncan C G. 1963. Role of microorganisms in weathering of wood and degradation of exterior finishes. Off Dig Fed Soc Paint Technol, 35: 1008-1012.
Erich S J, Adan O C, Pel L, et al. 2006. NMR Imaging of coatings on porous substrates. Chem Mater, 18: 4500-4504.
Feist W C. 1996. Painting and finishing exterior wood. Coat Technol, 68(856): 23-26.
Gething B A, Janowiak J J, Falk R H. 2009. Assessment of laser induced breakdown spectroscopy(LIBS)for classification of preservative in CCA-treated lumber. Forest Products Journal, 59: 67-74.
Gobakken L R, Hib O A, Solheim H. 2010. Mould growth on paints with different surface structures when applied on wooden claddings exposed outdoors. International Biodeterioration & Biodegradation, 64: 339-345.
Gobakken L R, Vestl G I. 2012. Surface mould and blue stain fungi on coated Norway spruce cladding. International Biodeterioration & Biodegradation, 75: 181-186.
Guseva O, Brunner S, Richner P. 2003. Service life prediction for aircraft coatings. Polym Degrad STab, 82 (1): 1-13.
Landry V, Blanchet P, Zotig L, et al. 2013. Performance of exterior semitransparent PVDF-acrylic coatings. Journal of Coatings Technology and Research, 10(1): 37-46.
Lawrence C, Van I. 2006. Wood finishing with UV-curable coatings. RADTECH REPORT: 32-38.
MacLeod I T, Scully A D, Ghiggino K P, et al. 1995. Photodegradation at the wood-clearcoat interface. Wood Science and Technology, 29: 183-189.
Manning D. 2003. The deal with decks. Painting & Wallcovering Contractor, 5, 3; ABI/INFORM Complete pg, 84.
Martin J W, Embree E, Tsao W. 1990. Non-osmotic defect controlled cathodic disbondment of a coating from a steel substrate. Journal of Coatings Technology, 62(790): 25-33.
Oosterbroek M, Lammers R J, Van de ven L. 1991. Crack formation and stress development in an organic coating. Coat Technol, 63(797): 55-60.
Pourmand P, Wang L V, Dvinskikh S V. 2011. Assessment of moisture protective properties of wood coatings by a portable NMR sensor. Journal of Coatings Technology and Research, 8(5): 649-654.
Prawoto Y, Onn I H. 2012. Modified Fourier solution for diffusion governing law applied to blister formation and development. Computational Materials Science, 62: 105-109.
Prestemon D, Sternweis L. 1994. Paint problems on exterior wood. Human Housing 5-2, Pm-363.
Sabani S, Onen A H, Gungor A. 2012.Preparation of hyperbranched polyester polyol-based urethane acrylates and applications on UV-curable wood coatings. Journal of Coatings Technology and Research, 9(6): 703-716.
Santana J J, Phler M, Souto R M, et al. 2012. Direct evidence of early blister formation in polymer-coated metals from exposure to chloride-containing electrolytes by alternating-current scanning electrochemical microscopy. Electrochimica Acta, 77: 60-64.
Singh A P, Dawson B. 2004. Confocal microscope——a valuable tool for examining wood-coating interface. JCT Research, 3: 235-237.
Singh A P, Ratz A, Dawson B. 2007. A novel method for high-resolution imaging of coating distribution within a rough-textured plywood surface. Journal of Coatings Technology and Research, 4(2): 207-210.
Singh A P, Dawson B S. 2003. The mechanism of failure of clear coated wooden boards as revealed by microscopy. IAWA Journal, 24(1): 1-11.
Solo-Gabriele H M, Townsend T G, Hahn D W, et al. 2004. Evaluation of XRF and LIBS technologies for on-line sorting of CCA-treated wood waste. Waste Management, 24(4): 413-424.
Tombaugh R S. 2009. Coating failures and misapplications in commercial painting. SSPC 2009 Conference Proceedings, 1-11.
Trumbo D L. 1996. Preliminary analysis of the 1H-NMR and 13 C-NMR spectra of poly(2,5-dimethyl-3-vinylfuran). Polymer Bulletin,37: 81-87.
Turkulin H, Arnold M, Derbyshire H, et al. 2001. Structural and fractographic SEM analysis of exterior coated wood. Surface Coatings International Part B. Coatings Transactions, 34: 67-75.
Vlad-Cristea M, Riedl B, Blanchet P, et al. 2012. Nanocharacterization techniques for investigating the durability of wood coatings. European Polymer Journal, 48: 441-453.
Westing E, Ferrari G M, Wit J. 1994. The determination of coating performance with impedance measurements—II. Water uptake of coatings. Corrosion Science, 36(6): 957-977.
Wikberg H. 2005. Advanced solid state NMR spectroscopic techniques in the study of thermally modified wood. Ph D Thesis,Faculty of Science of the University of Helsinki, Finland, 13-19.
Williams R S, Jourdain C, Daisey G I, et al. 2000. Wood properties affecting finish service life. Journal of Coatings Technology, 72: 35-42.
Williams R S, Winandy J E, Feist W C. 1987. Paint adhesion to weathered wood. Coat Technol, 59(749): 43-49.
Williams R S. 1983. Effect of grafted UV stabilizers on wood surface erosion and clear coating performance. Journal of Applied Polymer Science, 28: 2093-2103.
Williams R S. 2003. Effect of grafted UV stabilizers on wood surface erosion and clear coating performance. Journal of Applied Polymer Science, 28(6): 2093-2103.
Williams S, Knaebe M, Feist W. 1997. Why exterior finishes fail. Fine Homebuilding, 110: 61-65.
Xie Y J, Krause A, Militz H, et al. 2006. Coating performance of finishes on wood modified with an N-methylol compound. Progress in Organic Coatings, 291-300.
Yu J, Zheng R. 2012. Laser-induced plasma and laser-induced breakdown spectroscopy (LIBS) in China: The challenge and the opportunity. Front Phys, 7(6): 647-648. |