Growth and Wood Property of Poplar 741

Tian Xiaoming1, Xie Jin1, Qu Long1, Liu Shichang1, Li Jianmei1, Du Hongshuang2, Jiang Xiangning3, Gai Ying3   

  1. 1. College of Biological Sciences and Biotechnology, Beijing Forestry University Beijing 100083;2. Forestry College, Beihua University Jilin 132013;3. Tree and Ornamental Plant Breeding and Biotechnology Laboratory of State Forestry Administration National Engineering Laboratory for Tree Breeding Beijing 100083
  • Received:2012-05-28 Revised:2012-10-25 Online:2013-03-25 Published:2013-03-25

摘要: 对741杨的生长节律、细胞壁化学组成、解剖结构、物理力学性质进行观察和测定。结果表明: 741杨生长持续期长,生长速度快,株高、茎粗和单株材积生长量在生长旺季具有速生的特点; 在扫描电子显微镜下观察,741杨纤维细胞壁较薄,断面形状多为圆形或多边形,导管多为孔纹型导管,木射线为单列; 741杨茎细胞壁中S-木质素含量明显高于G-木质素,随着树龄的增加,S-木质素的含量逐年增加。741杨基本密度小于毛白杨成熟材,体积干缩率在杨属中处于较低水平,抗弯强度与同类型杨树木材相比处于较高水平,冲击韧性按我国主要用材树种冲击韧性大小的分类属中等。741杨可广泛应用于绿化、建筑、家具、胶合板、造纸等行业。

关键词: 741杨, 生长节律, 解剖结构, 化学组成, 物理力学性质

Abstract: Growth rhythm, cell wall composition, anatomical structure, physical and mechanical properties of poplar 741 were observed and measured. The results showed that, poplar 741 had a long growth period, high growth rate, and plant height, stem diameter and the growth rate of individual volume in growing season had the obvious characteristics of fast-growing. With the scanning electro microscope analysis, we found that fiber cell wall was thin, the shape of its cross section was circular or polygonal, the vessel cells were pitted vessel, wood rays were usually uniseriate; S-lignin content in stem cell wall of poplar 741 was markedly higher than the G-lignin, moreover, with the growing of the poplar 741, the S-lignin content increased year by year. Basic density of poplar 741 was less than Populus wood, volume shrinkage rate was in a low level, the flexural strength was higher than other kind of Populus wood. According to national standard of impact toughness in wood, the impact toughness of poplar 741 was medium among the main timber tree species. Poplar 741 could be widely applied in green, construction, furniture, plywood, paper and other industries.

Key words: poplar 741, growth rhythm, anatomical structure, chemical composition, physical and mechanical property